Appearance | White Paste |
Penetration | 170~300(1/10mm, 25℃) |
Specific Gravity | 2.7~3.0 |
Oil Separation | ≤1.0(%)(200℃, 8h) |
Volatile | ≤1.0(%)(200℃,8h) |
Breakdown Voltage Strength | ≥10(kv/mm) |
Volume Resistivity | ≥3×1014(Ω·CM) |
Thermal Conductivity | 3.8-4.2(w/m.k) |
1 kg/tank,10kg/barrel,80g/branch,150g/branch.
INSTRUCTIONS
Clean the surface of coated, the product can used to contact surface by smearing or roller coating by writing brush or silk-screen printing.
Metal Core PCB Thermal Conductivity 1-398W/m.K Aluminum/Copper AC 500-4000V Post-bonding/Pre-bonding Sweat-Soldering/Conductive Adhesive Press-Fit/Embedded Coin(I, T U) Founded in 2007,PEAK ...
GA-96*0 series thermal conductivity silicone rubber have good thermal conductive property, excellent heat transfer performance. Silicone rubber thermal properties GA-96*0 Series Heat Cure Rubber Feature: good thermal conductive property, good processability among thermally ...
Today ceramics are already widely used as substrates in many microelectronic components and power LED packages and more and more they are replacing entire printed circuit boards reducing complexity in design and manufacturing while increasing performance. Examples are ...
Thermal Conductive Insulating Fabric Tape with Silicone Adhesive Name : Conductive Fabric Tape Size: Width: Customized * 50m length Description: l Type: Anti electromagnetic radiation l Feature: Conductive fabric has excellent softness and excellent bending resistance, ...
ROHS Compliant: Yes UL recognized: Yes Features and Benefits: Thermal conductivity: 1~5.5 W/m·K Excellent thermal performance Good reliability Superior ability to flow and conform to interfaces Non-toxic, non-corrosive Application: 1. Power supply 2.Between a CPU and a heat ...
ZS-GF-5299 is a low viscosity two-component addition cure silicone sealant, that can be cured at room temperature or heat cure, the higher the temperature, the faster the curing. This product does not produce any byproducts in the curing reaction, which can be applied for PC ...
Appearance White Paste Penetration 170~300(1/10mm, 25℃) Specific Gravity 2.7~3.0 Oil Separation ≤1.0(%)(200℃, 8h) Volatile ≤1.0(%)(200℃,8h) Breakdown Voltage Strength ≥10(kv/mm) Volume Resistivity ≥3×1014(Ω·CM) Thermal Conductivity 3.8-4.2(w/m.k) 1 ...
Appearance White Paste Penetration 170~300(1/10mm, 25℃) Specific Gravity 2.7~3.0 Oil Separation ≤1.0(%)(200℃, 8h) Volatile ≤1.0(%)(200℃,8h) Breakdown Voltage Strength ≥10(kv/mm) Volume Resistivity ≥3×1014(Ω·CM) Thermal Conductivity 3.8-4.2(w/m.k) 1 ...