1.The light transmission of the sheet is quite good which is up to 85%.
|
|
|
|
|
|
|
|
2.The weather resistant treatment of anti UV on the surface of the sheet prevents the resin from turning yellow by causing Ultraviolet ray.
|
|
3.The UV agent has chemical bond to change ultraviolet ray into visible light, which has a stable effect on the photsynthesis of plants.
|
|
4.Its impact strength is 10 times of the ordinary ray glass, 3-5 times of the ordinary corrugated roofing sheet and 2 times of toughened glass. It is hardly broken.
|
|
5.Through the nationgal GV8625-88 test, its fire retardant is identified to be Grade 1, no fire drops nor toxic gas. In the temperature from -40C to 120C, the product will not deform.
|
|
6.It is light in weight, easy to handle and drill, convenient for construction and procession. When cutting for installation, it is not easy to be broken.
|